How To Find Activation Energy for Single-Step Curing Process From DSC experiments

Required:
1) NETZSCH Proteus Analysis software version 9.10 (or higher)
2) Kinetics Lite option 

Introduction

For kinetic analysis it is necessary to open in NETZSCH Protes Analysis software at least 3 experimental curves measured at different temperature conditions, more measurements are recommended. For DSC the segments with different heating rates or segments with different isothermal conditions are used for kinetic analysis.

This example presents the curing of epoxy resin.

Importing DSC Data from NETZSCH Proteus Analysis

  1. In NETZSCH Protes Analysis software open at least 3 experimental DSC curves measured at different temperature conditions
  2. For each experimental curve evaluate the peak area for the temperature (or time) range of interest. Please select the baseline, which is necessary for enthalpy evaluation. The evaluation ranges and the baselines can be different for different DSC curves.
  3. Select curves with peak area evaluation (click and ctrl+click on each curve or single click on DSC axis):

Figure 1. Proteus Analysis software with DSC data for kinetic analysis

 

4. In NETZSCH Protes Analysis select Kinetics Lite from Extras menu Item:

Figure 2. Selection of Kinetic Lite Option in NETZSCH Proteus Analysis software

 

Result: Kinetics Lite is started, where selected curves are automatically imported from Proteus Analysis into Kinetics Lite. Only selected ranges are loaded, baselines are subtracted, file names can be seen in Legend if File Name is selected in View ribbon:

Figure 3. Experimental curves are automatically loaded from Proteus Analysis into Kinetics Lite.

 

5. In Project Panel click on Add New to create single-step kinetic model.

Result: new single-step kinetic model is created. The reaction type is found automatically, for curing it is usually autocatalytic reaction of Cn type.

In the Properties panel you can find kinetic equation and kinetic parameters, including activation energy in kJ/mol. In the bottom of Properties Panel the fit quality R² can be found as well as the possibility to export kinetic equation with kinetic parameters to external txt file.

Figure 4. Experimental data (markers) and simulated curves for single-step kinetic model.